Hang samples of iron, steel, nickel, aluminium, copper, bismuth, plastic, wood and an unknown sample X in the non-uniform field of an electromagnet and measure the force with a sensor: ferromagnets are strongly attracted as their domains line up, paramagnets are weakly attracted and diamagnets weakly repelled, with the susceptibility χ shown. Heat iron or nickel and record the magnetisation against temperature to find the Curie temperature, where the domain order is lost. Sweep the field H to trace the hysteresis loops of soft iron and steel and read the remanence and coercivity.
Lesson: Magnetism and matter
What it shows
Every material responds to a magnetic field, but in three different ways. In ferromagnets such as iron, steel and nickel, atomic moments are already aligned in small regions called domains; a field makes the domains line up, so these metals are attracted very strongly. Paramagnets such as aluminium have atomic moments that line up only slightly, so they are weakly attracted (χ small and positive). Diamagnets such as copper, bismuth and water are weakly repelled, because the field induces moments that oppose it (χ negative). Heating a ferromagnet above its Curie temperature destroys the domain order and it becomes paramagnetic. A hysteresis loop shows why soft iron suits transformer cores and steel suits permanent magnets.
How to use
On Samples in a field, choose a Sample, set the Field B at the sample and press Record force; compare the size and sign of the force. On Curie point, choose the Metal, press Heat or move the Temperature slider, and press Record reading on both sides of the drop in M. On Hysteresis loop, choose the Material and press Cycle H, or move the Magnetising field H yourself, and press Record point. Tick Compare with the other material to see both loops.
Parameters you can change
- Starting screen Samples in a field, Curie point, Hysteresis loop
- Sample (Samples in a field screen) Iron, Steel, Nickel, Aluminium, Copper, Bismuth, Plastic (acrylic), Wood, Sample X
- Field B at the sample 0–1.5 T
- Metal (Curie point screen) Iron, Nickel
- Temperature (Curie point screen) 20–1000 °C
- Material (Hysteresis loop screen) Soft iron, Steel
Questions to explore
- Why is the force on bismuth opposite in direction to the force on aluminium?
- What happens to the magnetisation of nickel as it is heated past its Curie temperature?
- Why is steel better than soft iron for a permanent magnet?